Hot Pressed Boron Nitride | |||
Item | Unit | Index | |
Thermal Conductivity (RT) | W/m·k | 45-50 | |
Thermal expansivity (25-700℃) | 10-6/℃ | 6.5-7.5 | |
Resistivity (RT | Ω·m | >1012 | |
Puncture voltage | 106/kv·m | 2.5-4.0 | |
Mohs' hardness | 2 | ||
Dielectric constant (Σ) | 3.8-4.3 | ||
Bending strength (RT) | mpa | >35 | |
Compression strength (RT) | mpa | >200 | |
Density | g/cm3 | 1.9-2.2 | |
Chemical Composition | B+N | % | 99.5 |
Oxygen Content | % | <0.4 | |
Carbon Content | % | <0.05 | |
Working Environment Temperature | Oxidizing Atmosphere | ℃ | 900 |
Vacuum | ℃ | ≥2200 | |
Inertia | ℃ | ≥2200 | |
Pyrolytic Boron Nitride | |||
Item | Unit | Index | |
Lattice Constant | μm | a:2.504×10-10 c: 6.692×10-10 | |
Apparent Density | g/cm3 | 2.10–2.15(plate) 2.15–2.19(Crucible) | |
Helium Transmittance | cm3/s | 1×10-10 | |
Micro Hardness (Knoop)(ab flat) | N/mm2 | 691.88 | |
Volume Resistivity | Ω·cm | 3.11×1011 | |
Tensile Strength (Forcell “c”) | N/mm2 | 153.86 | |
Bending Strength | (Force || “C”) | N/mm2 | 243.63 |
(Force⊥ “C”) | N/mm2 | 197.76 | |
Elasticity Modulus | N/mm2 | 235690 | |
Thermal Conductivity | W/m·k | “a”direction “c”direction | |
(200℃) | W/m·k | 60 2.60 | |
(900℃) | W/m·k | 43.70 2.80 | |
Dielectric Strength(RT) | KV/mm | 56 | |